Adhesives used in machine building have to meet a large range of requirements. While high heat or chemical resistance are desirable for some applications, others may need special electrical properties or short curing cycles. With their outstanding property profiles, tailor-made ELASTOSIL®, SilGel® or SILRES® products master even the most sophisticated machine building requirements. What’s more, they are ecologically and physiologically safe and can also be used in food-contact applications on a case-by-case basis.

Properties:
- Heat resistance (up to 300 °C)
- Adhesion without pretreatment
- Chemical resistance
- Stable electrical properties
- Thermally conductive (from up to 2.5 W x K–1 x m–1)
- Radiation resistance (from microwave to UV range)
- Permanent elasticity (-45 °C to over 200 °C)
Product Recommendations
Products
|
Technical data
|
Product properties
|
|||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
Hardness Shore A | Tensile strength | Elongation at break | Viscosity, dynamic | Tear strength | Resistance | Regulation | Product Rheology | Crosslinking Property | Vulcanizate | ||
35[9] 35[9] | 2.5 N/mm²[11] 2.5 N/mm²[11] | 200 %[16] 200 %[16] | 25000 mPa·s[3] 25000 mPa·s[3] | 3.5 N/mm[1] 3.5 N/mm[1] | Heat resistant | - | - | - | - | ||
15[9] 15[9] | 0.8 N/mm²[11] 0.8 N/mm²[11] | 200 %[16] 200 %[16] | - - | - - | - | - | - | - | - | ||
28[9] 28[9] | 2.5 N/mm²[11] 2.5 N/mm²[11] | 300 %[16] 300 %[16] | 1000000 mPa·s[4] 1000000 mPa·s[4] | 7.8 N/mm[2] 7.8 N/mm[2] | Oil resistant | - | Non-slump | - | - | ||
20[9] 20[9] | 1.2 N/mm²[11] 1.2 N/mm²[11] | 300 %[16] 300 %[16] | 40000 mPa·s[5] 40000 mPa·s[5] | 3.0 N/mm[1] 3.0 N/mm[1] | Oil resistant, Heat resistant | - | Self-levelling | - | - | ||
25[9] 25[9] | 2.5 N/mm²[12] 2.5 N/mm²[12] | 300 %[17] 300 %[17] | - - | 8.0 N/mm[1] 8.0 N/mm[1] | Heat resistant | Solvent-free | Flowable | - | - | ||
32[9] 32[9] | 2.5 N/mm²[11] 2.5 N/mm²[11] | 400 %[16] 400 %[16] | - - | 7 N/mm[1] 7 N/mm[1] | Heat resistant | MIL-A 46106 grade | Non-slump | - | - | ||
30[9] 30[9] | 5 N/mm²[13] 5 N/mm²[13] | 400 %[18] 400 %[18] | - - | - - | - | Solvent-based | - | - | - | ||
15[9] 15[9] | 2 N/mm²[14] 2 N/mm²[14] | 750 %[19] 750 %[19] | - - | 7.3 N/mm[1] 7.3 N/mm[1] | - | - | Non-slump | - | - | ||
40[9] 40[9] | 6.0 N/mm²[14] 6.0 N/mm²[14] | 350 %[19] 350 %[19] | 100000 mPa·s[6] 100000 mPa·s[6] | 11.5 N/mm[1] 11.5 N/mm[1] | - | - | Self-levelling | - | - | ||
30[9] 30[9] | 6.5 N/mm²[15] 6.5 N/mm²[15] | 500 %[20] 500 %[20] | 250000 mPa·s[3] 250000 mPa·s[3] | 11.5 N/mm[1] 11.5 N/mm[1] | - | Solvent-free | - | - | - | ||
30[9] 30[9] | 7.5 N/mm²[11] 7.5 N/mm²[11] | 500 %[16] 500 %[16] | - - | - - | - | - | Thixotropic | - | - | ||
30[9] 30[9] | 7.8 N/mm²[11] 7.8 N/mm²[11] | 450 %[16] 450 %[16] | - - | - - | - | - | Thixotropic | - | - | ||
30[9] 30[9] | 6.50 N/mm²[14] 6.50 N/mm²[14] | 500 %[19] 500 %[19] | 250000 mPa·s[7] 250000 mPa·s[7] | 11.5 N/mm[1] 11.5 N/mm[1] | - | Solvent-free | - | - | - | ||
37[9] 37[9] | 4.5 N/mm²[15] 4.5 N/mm²[15] | 450 %[20] 450 %[20] | 600000 mPa·s[7] 600000 mPa·s[7] | 10 N/mm[1] 10 N/mm[1] | - | MIL-A 46106 grade | Non-slump, Thixotropic | - | - | ||
35[9] 35[9] | 2.6 N/mm²[11] 2.6 N/mm²[11] | 200 %[16] 200 %[16] | - - | - - | - | MIL-A 46106 grade | - | - | - | ||
30[9] 30[9] | 2.1 N/mm²[11] 2.1 N/mm²[11] | 200 %[16] 200 %[16] | - - | - - | - | - | - | - | - | ||
32[9] 32[9] | 3.0 N/mm²[11] 3.0 N/mm²[11] | 250 %[16] 250 %[16] | - - | - - | - | - | - | - | - | ||
32[9] 32[9] | 3.2 N/mm²[11] 3.2 N/mm²[11] | 250 %[16] 250 %[16] | - - | - - | - | - | - | - | - | ||
25[9] 25[9] | 1 N/mm²[12] 1 N/mm²[12] | 200 %[18] 200 %[18] | 10.000 mPa·s[8] 10.000 mPa·s[8] | - - | - | - | Shear thinning, Self-levelling | - | - | ||
35[9] 35[9] | 2 N/mm²[12] 2 N/mm²[12] | 200 %[18] 200 %[18] | 30000 mPa·s[7] 30000 mPa·s[7] | - - | - | Flame retardant | - | - | - | ||
36[9] 36[9] | 1.6 N/mm²[11] 1.6 N/mm²[11] | 150 %[16] 150 %[16] | - - | - - | - | Flame retardant | Flowable | - | - | ||
45[9] 45[9] | 1.5 N/mm²[12] 1.5 N/mm²[12] | 200 %[18] 200 %[18] | 250000 mPa·s[7] 250000 mPa·s[7] | 5.0 N/mm[1] 5.0 N/mm[1] | Oil resistant, Heat resistant | Flame retardant | Non-slump | - | - | ||
30[9] 30[9] | 2.5 N/mm²[12] 2.5 N/mm²[12] | 400 %[18] 400 %[18] | 950000 mPa·s[3] 950000 mPa·s[3] | 6.5 N/mm[1] 6.5 N/mm[1] | - | - | Non-slump | - | - | ||
30[9] 30[9] | 2.0 N/mm²[12] 2.0 N/mm²[12] | 450 %[17] 450 %[17] | 1000000 mPa·s[7] 1000000 mPa·s[7] | 8.5 N/mm[2] 8.5 N/mm[2] | - | Flame retardant | Non-slump, Thixotropic | - | - | ||
30[9] 30[9] | 2.2 N/mm²[12] 2.2 N/mm²[12] | 500 %[17] 500 %[17] | 1000000 mPa·s[7] 1000000 mPa·s[7] | 10 N/mm[2] 10 N/mm[2] | - | - | Non-slump, Thixotropic | - | - | ||
30[9] 30[9] | 2.20 N/mm²[12] 2.20 N/mm²[12] | 500 %[17] 500 %[17] | 900000 mPa·s[3] 900000 mPa·s[3] | 10 N/mm[2] 10 N/mm[2] | - | Flame retardant | Non-slump, Thixotropic | - | - | ||
40[9] 40[9] | 2.8 N/mm²[11] 2.8 N/mm²[11] | 300 %[16] 300 %[16] | - - | - - | Heat resistant | - | Shear thinning, Non-slump | - | - | ||
40[9] 40[9] | 6.1 N/mm²[11] 6.1 N/mm²[11] | 500 %[16] 500 %[16] | - - | 10.1[1] 10.1[1] | Heat resistant | - | Thixotropic | One-component | Self-adhesive | ||
- - | 5.9 N/mm²[11] 5.9 N/mm²[11] | 500 %[16] 500 %[16] | 600000 mPa·s[4] 600000 mPa·s[4] | 13.8 N/mm[1] 13.8 N/mm[1] | Media resistant, Heat resistant, UV stable | - | - | Fast curing under heat, Two-component, Addition Curing | - | ||
45[9] 45[9] | 1 N/mm²[11] 1 N/mm²[11] | 180 %[16] 180 %[16] | - - | - - | Media resistant | - | Shear thinning, Thixotropic | Condensation-curing, Two-component | Self-adhesive, Electrically insulating | ||
32[9] 32[9] | 2.0 N/mm²[11] 2.0 N/mm²[11] | 130 %[16] 130 %[16] | - - | 3.8 N/mm[1] 3.8 N/mm[1] | Heat resistant, Steam resistant | - | - | Condensation-curing, Two-component | Self-adhesive, Electrically insulating | ||
50[9] 50[9] | 3.5 N/mm²[11] 3.5 N/mm²[11] | 120 %[16] 120 %[16] | - - | 7.0[1] 7.0[1] | Heat resistant | - | Shear thinning, Non-slump | Condensation-curing, Two-component, Fast curing at room temperature | Self-adhesive, Electrically insulating | ||
50[10] 50[10] | 2.8 N/mm²[11] 2.8 N/mm²[11] | 250 %[16] 250 %[16] | - - | 9.5 N/mm[1] 9.5 N/mm[1] | Oil resistant | - | Shear thinning, Thixotropic, Non-slump | Condensation-curing, Two-component | Self-adhesive, Electrically insulating |
[1] Tear strength | ASTM D 624 B, [2] Tear strength | ASTM D 624 B | 23°C / 2mm, [3] Viscosity, dynamic D = 0,5 1/s | 25 °C | DIN EN ISO 3219, [4] Viscosity, dynamic | 25 °C | 0.5 1/s | DIN EN ISO 3219, [5] Viscosity, dynamic | 25 °C | DIN EN ISO 3219, [6] Viscosity, dynamic D = 1 1/s | 25 °C | DIN EN ISO 3219, [7] Viscosity, dynamic D = 0.5 1/s | 25 °C | DIN EN ISO 3219, [8] Viscosity, dynamic | 25 1/s | ISO 3219, [9] Hardness Shore A | DIN ISO 48-4, [10] Hardness Shore A | ISO 1183-1 A, [11] Tensile strength | ISO 37 type 1, [12] Tensile strength | ISO 37 | Type 3 / 23°C / 2mm, [13] Tensile strength | ISO 37 | Type 3 / 23 °C / d = 2 mm, [14] Tensile strength | ISO 37 type 1 | Type 3 / 23°C / 2mm, [15] Tensile strength | ISO 37 type 1 | Type 3 /23°C / 2mm, [16] Elongation at break | ISO 37 type 1, [17] Elongation at break | ISO 37 | Type 3 / 23°C / 2mm, [18] Elongation at break | ISO 37, [19] Elongation at break | ISO 37 type 1 | Type 3 / 23°C / 2mm, [20] Elongation at break | ISO 37 type 1 | Type 3 /23°C / 2mm, [] Suited, [] Well suited, [] Ideally suited